I was taught that cedar contains tanic acid and must be given a couple of months to “bleed” before a finish can be applied. I have a client that is upset that I did not back prime the clear cedar siding before installation. Any thoughts on this matter?
Discussion Forum
Discussion Forum
Up Next
Video Shorts
Featured Story

Low-e storm panels improve the energy efficiency of these old sash windows without changing their classic look.
Featured Video
Video: Build a Fireplace, Brick by BrickHighlights
"I have learned so much thanks to the searchable articles on the FHB website. I can confidently say that I expect to be a life-long subscriber." - M.K.
Replies
*
I was taught that cedar contains tanic acid and must be given a couple of months to "bleed" before a finish can be applied. I have a client that is upset that I did not back prime the clear cedar siding before installation. Any thoughts on this matter?